| Acrylonitrile Styrene Acrylate (ASA)
Processing Information |
Share This Page
• Free Access to 80,000 Datasheets
|
|
English
|
| Density (g/cm³) | 1.04 to 1.12 | 1.11 to 1.24 | 1.07 to 1.12 | | Mold Shrinkage, Flow (in/in) | 0.0050 to 0.0061 | 0.0049 to 0.0060 | 0.0040 to 0.0065 | | Melt Mass Flow Rate (g/10 min) | 0.20 to 2.0 | 0.50 to 35 | 5.0 to 11 | | Drying Temperature (°F) | 176 to 230 | 174 to 230 | 190 | | Drying Time (hr) | 2.9 to 4.1 | 3.0 to 4.0 | 4.0 | | Suggested Max Moisture (%) | 0.038 to 0.10 | 0.020 to 0.052 | 0.040 | | Suggested Max Regrind (%) | 5 to 30 | 5 to 6 | -- | | Injection Pressure (psi) | 9840 to 15200 | 14500 to 15200 | -- | | Rear Temperature (°F) | 391 to 476 | 418 to 477 | 451 | | Middle Temperature (°F) | 424 to 482 | 463 to 487 | 460 | | Front Temperature (°F) | 446 to 493 | 481 to 495 | 473 | | Nozzle Temperature (°F) | 419 to 503 | 454 to 491 | 460 | | Processing (Melt) Temp (°F) | 462 to 503 | 482 to 536 | 491 | | Mold Temperature (°F) | 131 to 163 | 140 to 176 | 163 |
SI
|
| Density (g/cm³) | 1.04 to 1.12 | 1.11 to 1.24 | 1.07 to 1.12 | | Mold Shrinkage, Flow (cm/cm) | 0.0050 to 0.0061 | 0.0049 to 0.0060 | 0.0040 to 0.0065 | | Melt Mass Flow Rate (g/10 min) | 0.20 to 2.0 | 0.50 to 35 | 5.0 to 11 | | Drying Temperature (°C) | 80.0 to 110 | 78.8 to 110 | 87.5 | | Drying Time (hr) | 2.9 to 4.1 | 3.0 to 4.0 | 4.0 | | Suggested Max Moisture (%) | 0.038 to 0.10 | 0.020 to 0.052 | 0.040 | | Suggested Max Regrind (%) | 5 to 30 | 5 to 6 | -- | | Injection Pressure (MPa) | 67.8 to 105 | 99.8 to 105 | -- | | Rear Temperature (°C) | 199 to 247 | 215 to 247 | 233 | | Middle Temperature (°C) | 218 to 250 | 239 to 253 | 238 | | Front Temperature (°C) | 230 to 256 | 249 to 257 | 245 | | Nozzle Temperature (°C) | 215 to 261 | 235 to 255 | 238 | | Processing (Melt) Temp (°C) | 239 to 262 | 250 to 280 | 255 | | Mold Temperature (°C) | 55.0 to 72.9 | 59.8 to 80.0 | 72.5 |
|
|