| Density (g/cm³) | 1.06 to 1.08 | | Mold Shrinkage, Flow (in/in) | 0.0035 to 0.0051 | | Melt Mass Flow Rate (g/10 min) | 0.70 to 26 | | Drying Temperature (°F) | 170 to 176 | | Drying Time (hr) | 1.9 to 4.0 | | Suggested Max Moisture (%) | 0.020 to 0.20 | | Suggested Max Regrind (%) | 20 | | Injection Pressure (psi) | 580 to 15000 | | Rear Temperature (°F) | 338 to 450 | | Middle Temperature (°F) | 389 to 450 | | Front Temperature (°F) | 413 to 467 | | Nozzle Temperature (°F) | 409 to 447 | | Processing (Melt) Temp (°F) | 400 to 483 | | Mold Temperature (°F) | 121 to 149 |
SI
|
| Density (g/cm³) | 1.06 to 1.08 | | Mold Shrinkage, Flow (cm/cm) | 0.0035 to 0.0051 | | Melt Mass Flow Rate (g/10 min) | 0.70 to 26 | | Drying Temperature (°C) | 76.7 to 80.1 | | Drying Time (hr) | 1.9 to 4.0 | | Suggested Max Moisture (%) | 0.020 to 0.20 | | Suggested Max Regrind (%) | 20 | | Injection Pressure (MPa) | 4.00 to 103 | | Rear Temperature (°C) | 170 to 232 | | Middle Temperature (°C) | 199 to 232 | | Front Temperature (°C) | 212 to 241 | | Nozzle Temperature (°C) | 209 to 230 | | Processing (Melt) Temp (°C) | 204 to 250 | | Mold Temperature (°C) | 49.2 to 64.9 |
|
|