| Styrene Maleic Anhydride (SMA)
Processing Information |
Share This Page
• Free Access to 80,000 Datasheets
|
|
English
|
| Density (g/cm³) | 1.06 to 1.17 | | Mold Shrinkage, Flow (in/in) | 0.0050 to 0.0061 | | Melt Mass Flow Rate (g/10 min) | 0.40 to 2.9 | | Drying Temperature (°F) | 170 to 194 | | Drying Time (hr) | 2.5 to 3.0 | | Suggested Max Moisture (%) | -- | | Suggested Max Regrind (%) | 20 | | Injection Pressure (psi) | -- | | Rear Temperature (°F) | 398 to 475 | | Middle Temperature (°F) | 421 to 485 | | Front Temperature (°F) | 450 to 495 | | Nozzle Temperature (°F) | 495 | | Processing (Melt) Temp (°F) | 449 to 500 | | Mold Temperature (°F) | 124 to 160 |
SI
|
| Density (g/cm³) | 1.06 to 1.17 | | Mold Shrinkage, Flow (cm/cm) | 0.0050 to 0.0061 | | Melt Mass Flow Rate (g/10 min) | 0.40 to 2.9 | | Drying Temperature (°C) | 76.7 to 90.0 | | Drying Time (hr) | 2.5 to 3.0 | | Suggested Max Moisture (%) | -- | | Suggested Max Regrind (%) | 20 | | Injection Pressure (MPa) | -- | | Rear Temperature (°C) | 203 to 246 | | Middle Temperature (°C) | 216 to 252 | | Front Temperature (°C) | 232 to 257 | | Nozzle Temperature (°C) | 257 | | Processing (Melt) Temp (°C) | 232 to 260 | | Mold Temperature (°C) | 51.1 to 71.1 |
|
|