The values listed as Molding Shrinkage, ISO 294-4, were tested in accordance with ISO 2577. Glass fiber content, ISO 3451-1: 10% Molding Shrinkage, ISO 2577, Across Flow, 150x105x3mm: 0.55 to 0.75% Molding Shrinkage, ISO 2577, Flow, 150x105x3mm: 0.3 to 0.5% Spiral flow length, Bayer test: 355 mm
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: Bayblend® DP T88 Plus, Bayblend DP T88 Plus, Bayblend® , Bayblend, BayblendDPT88Plus, DP T 88 Plus, DP T88 Plus, DPT, T88, 88Plus, DPT88Plus, Acrylonitrile Butadiene Styrene + PC, Acrylonitrile Butadiene Styrene PC, Acrylonitrile Butadiene Styrene : PC, Acrylonitrile Butadiene Styrene / PC, Acrylonitrile Butadiene Styrene - PC, Acrylonitrile Butadiene Styrene _ PC, Acrylonitrile Butadiene Styrene PC, ABS+PC, ABSPC, ABS:PC, ABS/PC, ABS-PC, ABS_PC, ABS PC, Acrylonitrile Butadiene Styrene, ABS, Bayer Euro, AcrylonitrileButadieneStyrenePC, AcrylonitrileButadieneStyrene, AcrylonitrileButadieneStyrene_PC, TDP
|