Product Description
Purging agent for injection molding machines
General  
Material Status 
  • Commercial: Active
Availability 
  • Asia Pacific
  • Europe
  • North America
Uses 
  • Purging Compound
Processing Method 
  • Injection Molding
Physical
Nominal Value
Unit
Test Method
Specific Gravity 2
     
--
 
ASTM D792
--
g/cm³
ISO 1183
Related Terminology
Product names can be difficult to match. You may have searched any one of these terms to find this product: RAMCLEAN™ 101, RAMCLEAN 101, RAMCLEAN™ , RAMCLEAN, RAMCLEAN101, 101, Thermoplastic, Unspecified, Thermoplastic Unspecified, TP, Unspecified, TP Unspecified, Polyram, ThermoplasticUnspecified, TPUnspecified
Injection Notes
Processing Instructions:

RAM-CLEAN is a Non-Corrosive, Non-Abrasive purging compound, based on pure physical effects of high-viscosity POLYOLEFINS, scrubbing MINERALS and FOAMING AGENTS.
The high viscosity polymer and the mineral filler will purge clean the surfaces of the cylinder, screw, nozzle and runners, removing residual polymers, pigments and other contaminants.
The foaming agents, while soaking for 5-10 minutes can penetrate into dead spots and help remove stubborn "sources" of black spots.
RAM-CLEAN works well with most polymers that are processed from 190 to 350 deg C.

1. CLEANING OF THE INJECTION UNIT (Cold runner Molds):
a. Heat the cylinder to normal processing temperatures. In some cases (such as shut-off nozzles, melt filters, mixers etc.) raise nozzle and front zone temperatures about 10 deg C above the production temperature.
b. Empty the cylinder from the current material by injection.
c. Increase the backpressure as much as possible and fill the cylinder with Ram-Clean 101 until foamed material emerges out of the machine nozzle.
d. Stop the screw rotation and let the system soak for about 5-10 minutes with the Ram-Clean inside the cylinder.
e. Empty the cylinder content.
f. If the last shot of the Ram-clean is still contains black specks or other contaminants, repeat stages c-d-e.
g. Set the temperature profile according to the next production material and purge the unit clean until there is no trace of Ram-Clean.

2. CLEANING THE HOT RUNNER SYSTEM
a. First clean the injection unit - steps a-b-c -mentioned above.
b. Raise hot runner temp to 20-30 deg above normal process temperature
c. Attach the injection unit to the mold and open the mold. Wait until foamed material emerges out of the hot nozzles- the foaming pressure is usually high enough to push the polymer out of the hot runner system.
d. If there is no flow out of the hot nozzles, reduce shot size to 50% and inject few half shots into a closed mold until the foamed Ram-Clean has reached the mold cavities.
e. Leave the mold open for 10 min, allowing the Ram-Clean to drool out of the hot nozzles. If you have shot-off nozzles leave them open!!
f. Same as in stage "d" reduce the shot weight to 50% and inject the whole cylinder content into the mold. Do not add any material until cylinder is fully purged.
g. Set hot runner temperatures to the next production temperatures.
h. Add the next production material and continue to inject half shots until there is no trace of the cleaning compound.
i. Set all parameters and start production.
Notes
1Typical properties: these are not to be construed as specifications.
2Bulk
 
IDES
Copyright © 2012 IDES
The information presented on this datasheet was acquired by IDES from the producer of the material. IDES makes substantial efforts to assure the accuracy of this data. However, IDES assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.