Product Description
DuPont™ Entira™ Strong 1002 is based on a copolymer of ethylene and methyl acrylate.

Entira™ Strong 1002 is used to modify the strength, toughness, and abrasion resistance of oriented PP, PET and PA. DuPont technical specialists are available by phone or email to further discuss application requirements and polymer selection.
General  
Material Status 
  • Commercial: Active
Availability 
  • Africa & Middle East
  • Asia Pacific
  • Europe
  • Latin America
  • North America
  • South America
Uses 
  • Blending
  • Fibers
  • Film
  • Tape
 
Forms 
  • Pellets
Processing Method 
  • Extrusion
Physical
Nominal Value
Unit
Test Method
Specific Gravity
     
--
 
ASTM D792
--
g/cm³
ISO 1183
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg)
g/10 min
ASTM D1238, ISO 1133
Thermal
Nominal Value
Unit
Test Method
Vicat Softening Temperature
°F
ISO 306/A50, ASTM D1525 2
Peak Melting Temperature
°F
ASTM D3418, ISO 3146
Related Terminology
Product names can be difficult to match. You may have searched any one of these terms to find this product: DuPont™ Entira™ Strong 1002, DuPont Entira Strong 1002, DuPont™ Entira™ , DuPont Entira, DuPontEntiraStrong1002, DuPontEntira, Strong 1002, Strong1002, Ethylene Methyl Acrylate Copolymer, EMA, Thermoplastic Elastomer, TPE, DuPont P&IP, EthyleneMethylAcrylateCopolymer, ThermoplasticElastomer, 1002Strong
Extrusion
Nominal Value
Unit
 
Melt Temperature
°F
 
Extrusion Notes
Entira™ Strong 1002 is available in pellet form for use in conventional extrusion equipment designed to process PP, PET, and PA resins.

Entira™ Strong 1002 can be fed together with base resin and other additives in the hopper during the fiber spinning or film/tape extrusion process. Typical addition levels of Entira™ Strong 1002 range from 2-10 wt%. If the temperature at the hopper exceeds 60-70°C (140-158°F), bridging may occur. Water cooling of the screw and/or hopper feed throat may help avoid bridging problems. As long as the melt temperature does not exceed 300°C (572°F), the extrusion processing conditions do not have to be altered when using Entira™ Strong 1002.
Notes
1Typical properties: these are not to be construed as specifications.
2Rate A (50°C/h), Loading 1 (10 N)
 
IDES
Copyright © 2012 IDES
The information presented on this datasheet was acquired by IDES from the producer of the material. IDES makes substantial efforts to assure the accuracy of this data. However, IDES assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.