Specific Gravity
|
|
|
|
|
--
|
|
|
ASTM D792 |
|
--
|
|
g/cm³
|
ISO 1183 |
|
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg)
|
|
g/10 min
|
ASTM D1238, ISO 1133 |
|
Molding Shrinkage
|
|
|
ASTM D955 |
|
Flow
|
|
in/in
|
|
|
Across Flow
|
|
in/in
|
|
|
Water Absorption (73°F, 24 hr)
|
|
%
|
ASTM D570, ISO 62 |
|
Tensile Strength (Yield)
|
|
psi
|
ASTM D638, ISO 527-2 |
|
Tensile Elongation (Break)
|
|
%
|
ASTM D638, ISO 527-2 |
|
Flexural Modulus
|
|
psi
|
ASTM D790, ISO 178 |
|
Notched Izod Impact
|
|
|
|
|
-4°F
|
|
ft·lb/in
|
ASTM D256, ISO 180 |
|
32°F
|
|
ft·lb/in
|
ISO 180, ASTM D256 |
|
73°F
|
|
ft·lb/in
|
ASTM D256, ISO 180 |
|
Deflection Temperature Under Load (264 psi, Unannealed)
|
|
°F
|
ASTM D648, ISO 75-2/A |
|
Vicat Softening Temperature
|
|
|
|
|
--
|
|
°F
|
ASTM D1525 2, ISO 306/A 2 |
|
--
|
|
°F
|
ASTM D1525 3, ISO 306/B 3 |
|
Ball Pressure Test (257°F)
|
|
|
VDE 0470 |
|
CLTE - Flow
|
|
in/in/°F
|
ASTM D696 |
|
Comparative Tracking Index (Solution A)
|
|
V
|
IEC 60112 |
|
Flame Rating - UL (0.0630 in)
|
|
|
UL 94 |
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: HAIPLEN EP70 C8, HAIPLEN , HAIPLENEP70C8, EP 70 C 8, EP70 C8, EP70, 70C, C8, EP70C8, Polypropylene Copolymer, PP Copolymer, Polypropylene, PP, Taro Plast, PolypropyleneCopolymer, PPCopolymer, 70EP
|
|