SCHULAMID® 12 GF 20 H

Polyamide 12

Glass Fiber Reinforcement, 20%

Supplied by A. Schulman Europe

The technical datasheet with complete property values for SCHULAMID® 12 GF 20 H is available to members of the Prospector Plastics Database.
Register to view full datasheet.
Register to View Full Datasheet
Product Description
20% glass fiber reinforced and heat stabilized Polyamide 12
General  
Material Status 
  • Commercial: Active
Availability 
  • Africa & Middle East
  • Asia Pacific
  • Europe
  • Latin America
  • North America
  • South America
Filler / Reinforcement 
  • Glass Fiber Reinforcement, 20% Filler by Weight
Features 
  • Balanced Stiffness/Toughness
  • Fuel Resistant
  • Good Chemical Resistance
  • Good Corrosion Resistance
  • Good Dimensional Stability
  • Good Heat Aging Resistance
  • Good Processability
  • Low to No Water Absorption
  • Oil Resistant
Processing Method 
  • Injection Molding
Physical
Dry
Conditioned
Unit
Test Method
Density
--
g/cm³
ISO 1183/A
Mechanical
Dry
Conditioned
Unit
Test Method
Tensile Modulus
psi
ISO 527-2/1A/1
Tensile Stress (Break)
psi
ISO 527-2/1A/5
Tensile Strain (Break)
%
ISO 527-2/1A/5
Impact
Dry
Conditioned
Unit
Test Method
Charpy Notched Impact Strength
      ISO 179/1eA
-22°F
--
ft·lb/in²
 
73°F
ft·lb/in²
 
Charpy Unnotched Impact Strength
      ISO 179/1eU
-22°F
--
ft·lb/in²
 
73°F
ft·lb/in²
 
Thermal
Dry
Conditioned
Unit
Test Method
Heat Deflection Temperature
       
66 psi, Unannealed
--
°F
ISO 75-2/Bf
264 psi, Unannealed
--
°F
ISO 75-2/Af
Vicat Softening Temperature
       
--
--
°F
ISO 306/A50
--
--
°F
ISO 306/B50
Electrical
Dry
Conditioned
Unit
Test Method
Comparative Tracking Index (Solution A)
--
V
IEC 60112
Flammability
Dry
Conditioned
Unit
Test Method
Burning Rate (0.0787 in)
--
in/min
ISO 3795
Flammability Classification
      IEC 60695-11-10, -20
0.0591 in
--
 
 
0.118 in
--
 
 
Glow Wire Flammability Index
      IEC 60695-2-12
0.0591 in
--
°F
 
0.118 in
--
°F
 
Glow Wire Ignition Temperature
      IEC 60695-2-13
0.0591 in
--
°F
 
0.118 in
--
°F
 
Related Terminology
Dry
Product names can be difficult to match. You may have searched any one of these terms to find this product: SCHULAMID® 12 GF 20 H, SCHULAMID 12 GF 20 H, SCHULAMID® , SCHULAMID, SCHULAMID12GF20H, 12 GF 20 H, 12GF, GF20, 20H, 12GF20H, Polyamide 12, Nylon 12, Polyamide, Nylon, pa12, A. Schulman Eur, Polyamide12, Nylon12, GF12
Generic Name
Dry
Generic Name may also be described by the following terms: PA12.
Conditioned
Generic Name may also be described by the following terms: PA12.
Features
Dry
Features may also be described by the following terms: Good Heat Aging Resistance, Good Dimensional Stability, Dimensionally Stable, Good Corrosion Resistance, Corrosion Resistant, Good Chemical Resistance, Chemical Resistant, Good Stiffness/Toughness Balance, Balanced Stiffness/Toughness, Good Processability, Easy Processing, Low Water Absorption, Low Moisture Absorption, Water Resistant, Moisure Resistant.
Conditioned
Product names can be difficult to match. You may have searched any one of these terms to find this product: SCHULAMID® 12 GF 20 H, SCHULAMID 12 GF 20 H, SCHULAMID® , SCHULAMID, SCHULAMID12GF20H, 12 GF 20 H, 12GF, GF20, 20H, 12GF20H, Polyamide 12, Nylon 12, Polyamide, Nylon, pa12, A. Schulman Eur, Polyamide12, Nylon12, GF12
Notes
1Typical properties: these are not to be construed as specifications.
 
IDES
Copyright © 2012 IDES
The information presented on this datasheet was acquired by IDES from the producer of the material. IDES makes substantial efforts to assure the accuracy of this data. However, IDES assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.