Flame Resistance, Ignition time, ASTM D229-11: 83 sec Flame Resistance, Burning time, ASTM D229-11: 221 sec Temperature class: 155°C Bond Strength, ASTM D-229, 0.5 in: 2000 psi
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: Haysite Plastics EHC, Haysite Plastics , HaysitePlasticsEHC, HaysitePlastics, PlasticsEHC, Plastics, EHC, Polyester, Thermoset, Polyester Thermoset, Polyester, TS, Polyester TS, Thermoset, TS, Haysite, PolyesterThermoset, PolyesterTS
|
|
This plastic material has 4 certifications from the following agencies (the number in parentheses shows the number of certifications for that agency): MIL (1), IEEE (1), FED (1), NEMA (1).
|