Already have an account?
Login Here
IDES
FORMION® FI 393
Ionomer
Glass Fiber Reinforcement, 10%
Supplied by A. Schulman Inc.
The technical datasheet with complete property values for FORMION® FI 393 is available to members of the
Prospector Plastics Database
.
Register to view full datasheet
.
Register to View Full Datasheet
Product Description
Ionomer HDPE 13% Glass Fiber
General
Material Status
Commercial: Active
Availability
North America
Filler / Reinforcement
Glass Fiber Reinforcement, 10% Filler by Weight
Physical
Nominal Value
Unit
Test Method
Density
g/cm³
ISO 1183/A
Mechanical
Nominal Value
Unit
Test Method
Tensile Stress
(Yield, 73°F)
psi
ISO 527-2/1A/50
Flexural Modulus - Chord
2
(73°F)
psi
ISO 178
Impact
Nominal Value
Unit
Test Method
Notched Izod Impact Strength
(73°F, Complete Break)
ft·lb/in²
ISO 180/1A
Related Terminology
Product names can be difficult to match. You may have searched any one of these terms to find this product: FORMION® FI 393, FORMION FI 393, FORMION® , FORMION, FORMIONFI393, FI 393, FI393, Ionomer, A. Schulman, 393FI
Notes
1
Typical properties: these are not to be construed as specifications.
2
Type 1A, 2.0 in/min
Copyright © 2012
IDES
The information presented on this datasheet was acquired by IDES from the producer of the material. IDES makes substantial efforts to assure the accuracy of this data. However, IDES assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.