Density
|
|
--
|
g/cm³
|
ISO 1183 |
|
Water Absorption (Saturation, 73°F)
|
|
--
|
%
|
ISO 62 |
|
Tensile Modulus
|
|
|
psi
|
ISO 527-2 |
|
Tensile Stress (Break)
|
|
|
psi
|
ISO 527-2 |
|
Tensile Strain (Break)
|
|
|
%
|
ISO 527-2 |
|
Flexural Modulus
|
|
|
psi
|
ISO 178 |
|
Charpy Notched Impact Strength
|
|
|
|
ISO 179/1eA |
|
-22°F
|
--
|
|
ft·lb/in²
|
|
|
73°F
|
--
|
|
ft·lb/in²
|
|
|
Charpy Unnotched Impact Strength
|
|
|
|
ISO 179/1eU |
|
-22°F
|
--
|
|
|
|
|
73°F
|
--
|
|
|
|
|
Heat Deflection Temperature (264 psi, Unannealed)
|
|
--
|
°F
|
ISO 75-2/A |
|
Melting Temperature
|
|
--
|
°F
|
ISO 11357-2 |
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: Hiprolon® 400 FN, Hiprolon 400 FN, Hiprolon® , Hiprolon, Hiprolon400FN, 400 FN, 400FN, Polyamide, Unspecified, Polyamide Unspecified, Nylon, Unspecified, Nylon Unspecified, Polyamide, Nylon, Suzhou Hipro Polymers, PolyamideUnspecified, NylonUnspecified, FN400
|
|
|
Features may also be described by the following terms: Low Density, Low Specific Gravity, Low Water Absorption, Low Moisture Absorption, Water Resistant, Moisure Resistant, Good Chemical Resistance, Chemical Resistant, High Impact Resistance.
|
|
|
Uses may also be described by the following terms: Monofilaments, Monofilament, Compounding, Compounds.
|
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: Hiprolon® 400 FN, Hiprolon 400 FN, Hiprolon® , Hiprolon, Hiprolon400FN, 400 FN, 400FN, Polyamide, Unspecified, Polyamide Unspecified, Nylon, Unspecified, Nylon Unspecified, Polyamide, Nylon, Suzhou Hipro Polymers, PolyamideUnspecified, NylonUnspecified, FN400
|