Density
|
|
g/cm³
|
ISO 1183 |
|
Melt Volume-Flow Rate (MVR) (260°C/2.16 kg)
|
|
in³/10min
|
ISO 1133 |
|
Water Absorption
|
|
|
ISO 62 |
|
Saturation, 73°F
|
|
%
|
|
|
Equilibrium, 73°F, 50% RH
|
|
%
|
|
|
Tensile Modulus
|
|
psi
|
ISO 527-2/1 |
|
Tensile Strength
|
|
|
|
|
Yield 2
|
|
psi
|
ASTM D638 |
|
Break 2
|
|
psi
|
ASTM D638 |
|
Break
|
|
psi
|
ISO 527-2/50 |
|
Tensile Elongation
|
|
|
|
|
Yield 3
|
|
%
|
ASTM D638 |
|
Yield 2
|
|
%
|
ASTM D638 |
|
Break 3
|
|
%
|
ASTM D638 |
|
Break 2
|
|
%
|
ASTM D638 |
|
Break
|
|
%
|
ISO 527-2/5, ISO 527-2/50 |
|
Flexural Modulus 4
|
|
psi
|
ISO 178 |
|
Flexural Strength 4, 5
|
|
psi
|
ISO 178 |
|
Notched Izod Impact Strength 6
|
|
|
ISO 180/1A |
|
-22°F
|
|
ft·lb/in²
|
|
|
32°F
|
|
ft·lb/in²
|
|
|
73°F
|
|
ft·lb/in²
|
|
|
Heat Deflection Temperature 7
|
|
|
|
|
66 psi, Unannealed, 3.94 in Span
|
|
°F
|
ISO 75-2/Be |
|
264 psi, Unannealed, 3.94 in Span
|
|
°F
|
ISO 75-2/Ae |
|
Vicat Softening Temperature
|
|
|
|
|
--
|
|
°F
|
ISO 306/A50 |
|
--
|
|
°F
|
ISO 306/B50 |
|
--
|
|
°F
|
ISO 306/B120 |
|
Ball Pressure Test (167°F)
|
|
|
IEC 60695-10-2 |
|
CLTE - Flow (-22 to 176°F)
|
|
in/in/°F
|
ISO 11359-2 |
|
This supplier and product may also be known by these terms: GE Plastics, LNP Engineering Plastics
Product names can be difficult to match. You may have searched any one of these terms to find this product: GELOY* HRA222 Resin, GELOY HRA222 Resin, GELOY* , GELOY, GELOYHRA222Resin, HRA 222 Resin, HRA222 Resin, HRA222, 222Resin, HRA222Resin, Acrylonitrile Styrene Acrylate, ASA, SABIC IP Asia, AcrylonitrileStyreneAcrylate, 222HRA
|
|
Features may also be described by the following terms: Bromine Free, No Bromine Content, No Chlorine Content, Chlorine Free, Good UV Resistance, UV Resistant, Ultraviolet Resistant, Ultraviolet Light Resistant.
|
|
Uses may also be described by the following terms: Electrical Applications, Electronic Applications, Electrical/Electronic Applications, Electrical Sector.
|