Product Description
Heat-stabilized, impact-modified, glass fiber-reinforced molding compound based on nylon 612 especially suitable for plastic and EPDM-rubber composites

VESTAMID DX9324 is a black pigmented glass fiber-reinforced, impact-modified PA 612 compound. The material contains about 35% glass fibers, an ageing protective agent and processing aid for a fast and even form filling. VESTAMID DX9324 is especially suitable for the production of plastic and rubber composites. This process is patented by Evonik Degussa GmbH.

Parts of VESTAMID DX9324 can also be bonded to EPDM-rubber without using any adhesives or adhesion promoters.

Because of its semi-crystalline morphology VESTAMID DX9324 provides an excellent chemical resistance, e.g., against greases, oils, fuels and hydraulic fluids.
General  
Material Status 
  • Commercial: Active
Availability 
  • Europe
  • North America
 
Filler / Reinforcement 
  • Glass Fiber Reinforcement, 35% Filler by Weight
Additive 
  • Heat Stabilizer
  • Impact Modifier
  • Processing Aid
Features 
  • Bondability
  • Fuel Resistant
  • Gasoline Resistance
  • Good Chemical Resistance
  • Good Processability
  • Grease Resistant
  • Heat Stabilized
  • Impact Modified
  • Oil Resistant
Uses 
  • Bonding
  • Compounding
 
Appearance 
  • Black
Forms 
  • Pellets
Processing Method 
  • Compounding
Physical
Nominal Value
Unit
Test Method
Density
g/cm³
ISO 1183
Molding Shrinkage
    ISO 294-4
Across Flow: 176°F, 0.0787 in 2
%
 
Across Flow: 248°F, 0.0787 in 3
%
 
Flow: 176°F, 0.0787 in 2
%
 
Flow: 248°F, 0.0787 in 3
%
 
Mechanical
Nominal Value
Unit
Test Method
Tensile Modulus
psi
ISO 527-2
Tensile Stress (Yield)
psi
ISO 527-2
Tensile Strain (Break)
%
ISO 527-2
Impact
Nominal Value
Unit
Test Method
Charpy Notched Impact Strength
    ISO 179/1eA
-22°F, Complete Break
ft·lb/in²
 
73°F, Complete Break
ft·lb/in²
 
Charpy Unnotched Impact Strength
    ISO 179/1eU
-22°F, Complete Break
ft·lb/in²
 
73°F, Complete Break
ft·lb/in²
 
Thermal
Nominal Value
Unit
Test Method
Heat Deflection Temperature
     
66 psi, Unannealed
°F
ISO 75-2/B
264 psi, Unannealed
°F
ISO 75-2/A
Electrical
Nominal Value
Unit
Test Method
Surface Resistivity
ohm
IEC 60093
Related Terminology
Product names can be difficult to match. You may have searched any one of these terms to find this product: VESTAMID® DX9324, VESTAMID DX9324, VESTAMID® , VESTAMID, VESTAMIDDX9324, DX 9324, DX9324, Polyamide 612, Nylon 612, Polyamide, Nylon, pa612, Evonik Degussa, Polyamide612, Nylon612, 9324DX
Generic Name
Generic Name may also be described by the following terms: PA612, PA6/12.
Features
Features may also be described by the following terms: Heat Stabilized, Heat-ageing Stabilized, Heat Ageing Stabilized, Heat-aging Stabilized, Heat Aging Stabilized, Good Chemical Resistance, Chemical Resistant, Good Processability, Easy Processing, Bondability, Bondable.
Uses
Uses may also be described by the following terms: Compounding, Compounds.
Notes
1Typical properties: these are not to be construed as specifications.
2determined on 2 mm sheetsvwith film gate at rim mold temperature 80°C
3Post Shrink, determined on 2 mm sheets with film gate at rim after 5 h heat aging at 120°C
 
IDES
Copyright © 2012 IDES
The information presented on this datasheet was acquired by IDES from the producer of the material. IDES makes substantial efforts to assure the accuracy of this data. However, IDES assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.