IDES Prospector Already have an account? Login Here

IDES

Arnite® AV2 360 S

Polyethylene Terephthalate

Glass Fiber Reinforcement, 33%

Supplied by DSM Engineering Plastics

The technical datasheet with complete property values for Arnite® AV2 360 S is available to members of the Prospector Plastics Database.
Register to view full datasheet.
Register to View Full Datasheet
General  
Material Status 
  • Commercial: Active
Availability 
  • Europe
Filler / Reinforcement 
  • Glass Fiber Reinforcement, 33% Filler by Weight
Additive 
  • Flame Retardant
  • Mold Release
 
Features 
  • Flame Retardant
RoHS Compliance 
Forms 
  • Pellets
Processing Method 
  • Injection Molding
Multi-Point Data 
  • Isochronous Stress vs. Strain (ISO 11403-1)
  • Isothermal Stress vs. Strain (ISO 11403-1)
  • Secant Modulus vs. Strain (ISO 11403-1)
  • Shear Modulus vs. Temperature (ISO 11403-1)
  • Viscosity vs. Shear Rate (ISO 11403-2)
Physical
Nominal Value
Unit
Test Method
Density
     
--
g/cm³
ISO 1183
--
lb/in³
ISO 1183 2
Molding Shrinkage
    ISO 2577 2
Flow
%
 
Across Flow
%
 
Water Absorption
     
Saturation, 73°F
%
ISO 62
Saturation
%
ISO 62 2
Equilibrium, 73°F, 50% RH
%
ISO 62
Equilibrium
%
ISO 62 2
Mechanical
Nominal Value
Unit
Test Method
Tensile Modulus
psi
ISO 527-2
Tensile Stress (Break)
psi
ISO 527-2
Tensile Strain (Break)
%
ISO 527-2
Impact
Nominal Value
Unit
Test Method
Charpy Notched Impact Strength
     
-22°F
ft·lb/in²
ISO 179/1eA
73°F
ft·lb/in²
ISO 179/1eA
-22°F
ft·lb/in²
ISO 179/1eA 2
73°F
ft·lb/in²
ISO 179/1eA 2
Charpy Unnotched Impact Strength
     
-22°F
ft·lb/in²
ISO 179/1eU
73°F
ft·lb/in²
ISO 179/1eU
-22°F
ft·lb/in²
ISO 179/1eU 2
73°F
ft·lb/in²
ISO 179/1eU 2
Thermal
Nominal Value
Unit
Test Method
Heat Deflection Temperature
     
66 psi, Unannealed
°F
ISO 75-2/B
66 psi
°F
ISO 75-2 2
264 psi, Unannealed
°F
ISO 75-2/A
264 psi
°F
ISO 75-2 2
Melting Temperature 3
°F
ISO 11357-3 2
CLTE
    ISO 11359-2
Flow
in/in/°F
 
Transverse
in/in/°F
 
Electrical
Nominal Value
Unit
Test Method
Surface resistivity
ohms
IEC 60093 2
Volume Resistivity
     
--
ohm·cm
IEC 60093
--
ohm·in
IEC 60093 2
Relative Permittivity
    IEC 60250
100 Hz
 
 
1 MHz
 
 
Dissipation Factor
    IEC 60250
100 Hz
 
 
1 MHz
 
 
Comparative Tracking Index
     
--
V
IEC 60112
--
 
IEC 60112 2
Electric Strength
V/mil
IEC 60243-1
Flammability
Nominal Value
Unit
Test Method
Burning Behav. at 1.6mm nom. thickn. (0.06 in, UL)
 
ISO 1210 2
Burning Behav. at thickness h (0.0280 in, UL)
 
ISO 1210 2
Flammability Classification
    IEC 60695-11-10, -20
0.0280 in
 
 
0.0591 in
 
 
Oxygen Index
%
ISO 4589-2
Related Terminology
Product names can be difficult to match. You may have searched any one of these terms to find this product: Arnite® AV2 360 S, Arnite AV2 360 S, Arnite® , Arnite, ArniteAV2360S, AV 2 360 S, AV2 360 S, AV2, 2360, 360S, AV2360S, Polyethylene Terephthalate, PET, Polyester, DSM EP, PolyethyleneTerephthalate, 2AV
Injection
Nominal Value
Unit
 
Drying Temperature
°F
 
Drying Time
hr
 
Suggested Max Moisture
%
 
Rear Temperature
°F
 
Middle Temperature
°F
 
Front Temperature
°F
 
Nozzle Temperature
°F
 
Processing (Melt) Temp
°F
 
Mold Temperature
°F
 
Notes
1Typical properties: these are not to be construed as specifications.
2Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted.
318 °F/min
 
IDES
Copyright © 2012 IDES
The information presented on this datasheet was acquired by IDES from the producer of the material. IDES makes substantial efforts to assure the accuracy of this data. However, IDES assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.