vs. Metal - Dynamic, Extrusion Coating
|
|
|
|
|
vs. Metal - Static, Extrusion Coating
|
|
|
|
|
Yield: 40800 in²/lb Tensile Strength @ Break, ASTM D 882, MD: 34000 to 38000 psi Tensile Strength @ Break, ASTM D 882, TD: 34000 to 38000 psi Elongation @ Break, ASTM 882, MD: 75 to 100% Elongation @ Break, ASTM 882, TD: 75 to 100% Secant Modulus, ASTM D 882, MD: 300000 to 375000 psi Secant Modulus, ASTM D 882, TD: 275000 to 350000 psi Graves Tear (initial), ASTM D 1004, MD: 1100 to1400 g/mil Graves Tear (initial), ASTM D 1004, TD: 1100 to1400 g/mil Coefficient of Friction, ASTM D 1894: 0.6 to 0.7 vs Itself-Dynamic Coefficient of Friction, ASTM D 1894: 0.9 to 1.3 vs Itself-Static Coefficient of Friction, ASTM D 1894: 0.2 to 0.4 vs Metal-Dynamic Coefficient of Friction, ASTM D 1894: 0.3 to 0.5 vs Metal-Static Coefficient of Friction, ASTM D 1894, Extrusion Coated: 0.4 to 0.7 vs Metal-Dynamic Coefficient of Friction, ASTM D 1894, Extrusion Coated: 0.8 to 1.8 vs Metal-Static Dimensional Stability, ASTM D1204, MD, 320°F, 5min: < 2.5% shrinkage Dimensional Stability, ASTM D1204, TD, 320°F, 5min: <1.5% shrinkage
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: OxyShield® 1545, OxyShield 1545, OxyShield® , OxyShield, OxyShield1545, 1545, Polyamide 6, Nylon 6, Polyamide, Nylon, pa6, Honeywell, Polyamide6, Nylon6
|