Density
|
|
lb/in³
|
ISO 1183 2 |
|
Melt Mass-Flow Rate (MFR) (300°C/1.2 kg)
|
|
g/10 min
|
ISO 1133 |
|
Melt volume-flow rate (300°C/1.2 kg)
|
|
in³/10min
|
ISO 1133 2 |
|
Molding Shrinkage - Flow
|
|
%
|
ISO 294-4 |
|
Water Absorption
|
|
|
ISO 62 |
|
73°F, 24 hr
|
|
%
|
|
|
Equilibrium, 73°F, 50% RH
|
|
%
|
|
|
Tensile Modulus
|
|
psi
|
ISO 527-2/50, ISO 527-2 2 |
|
Tensile Stress
|
|
|
|
|
Yield
|
|
psi
|
ISO 527-2/50, ISO 527-2 2 |
|
Break
|
|
psi
|
ISO 527-2/50 |
|
Tensile Strain
|
|
|
|
|
Yield
|
|
%
|
ISO 527-2/50, ISO 527-2 2 |
|
Break
|
|
%
|
ISO 527-2/50 |
|
Nominal strain at break
|
|
%
|
ISO 527-2 2 |
|
Flexural Modulus 3
|
|
psi
|
ISO 178 |
|
Flexural Strength 3
|
|
psi
|
ISO 178 |
|
Charpy notched impact strength
|
|
|
ISO 179/1eA 2 |
|
-22°F
|
|
ft·lb/in²
|
|
|
73°F
|
|
ft·lb/in²
|
|
|
Charpy impact strength
|
|
|
ISO 179/1eU 2 |
|
-22°F
|
|
|
|
|
73°F
|
|
|
|
|
Notched Izod Impact Strength (73°F)
|
|
ft·lb/in²
|
ISO 180/A |
|
Rockwell Hardness
|
|
|
ISO 2039-2 |
|
M-Scale
|
|
|
|
|
R-Scale
|
|
|
|
|
Heat Deflection Temperature
|
|
|
|
|
66 psi, Annealed
|
|
°F
|
ISO 75-2/B |
|
66 psi
|
|
°F
|
ISO 75-2 2 |
|
264 psi, Unannealed
|
|
°F
|
ISO 75-2/A |
|
264 psi, Annealed
|
|
°F
|
ISO 75-2/A |
|
264 psi
|
|
°F
|
ISO 75-2 2 |
|
Vicat Softening Temperature
|
|
|
|
|
--
|
|
°F
|
ISO 306/B50 |
|
50°C/h, B (50N)
|
|
°F
|
ISO 306 2 |
|
Ball Indentation Temperature
|
|
°F
|
IEC 60335-1 |
|
CLTE - Flow
|
|
in/in/°F
|
ISO 11359-2 2 |
|
Volume resistivity
|
|
ohm·in
|
IEC 60093 2 |
|
Dielectric Constant
|
|
|
|
|
60 Hz
|
|
|
IEC 60250 |
|
1 MHz
|
|
|
ASTM D150, IEC 60250 2 |
|
100 Hz
|
|
|
IEC 60250 2 |
|
Dissipation Factor
|
|
|
|
|
50 Hz
|
|
|
IEC 60250 |
|
1 MHz
|
|
|
ASTM D150, IEC 60250 2 |
|
100 Hz
|
|
|
IEC 60250 2 |
|
Comparative Tracking Index (0.0787 in, Solution A)
|
|
V
|
IEC 60112 |
|
Electric strength
|
|
V/mil
|
IEC 60243-1 2 |
|
Flame Rating - UL 4
|
|
|
UL 94 |
|
0.118 in
|
|
|
|
|
0.0295 in
|
|
|
|
|
0.0591 in
|
|
|
|
|
Burning Behav. at 1.6mm nom. thickn. (0.06 in, UL)
|
|
|
ISO 1210 2 |
|
Burning Behav. at thickness h (0.126 in, UL)
|
|
|
ISO 1210 2 |
|
Glow Wire Flammability Index
|
|
|
IEC 60695-2-12 |
|
0.0394 in
|
|
°F
|
|
|
0.0787 in
|
|
°F
|
|
|
0.118 in
|
|
°F
|
|
|
Glow Wire Ignition Temperature
|
|
|
IEC 60695-2-13 |
|
0.0394 in
|
|
°F
|
|
|
0.0787 in
|
|
°F
|
|
|
0.118 in
|
|
°F
|
|
|
Oxygen index
|
|
%
|
ISO 4589-2 2 |
|
Refractive Index
|
|
|
ISO 489 |
|
Transmittance
|
|
%
|
ASTM D1003 |
|
Haze
|
|
%
|
ASTM D1003 |
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: CALIBRE™ 301-10, CALIBRE 30110, CALIBRE™ , CALIBRE, CALIBRE30110, 301, 301-10, 30110, 301:10, 301/10, 301+10, 301_10, 301 10, Polycarbonate, PC, Styron, 10301
|
|
This plastic material has 2 certifications from the following agencies (the number in parentheses shows the number of certifications for that agency): CSA (1), UL (1).
|