IDES Prospector Already have an account? Login Here

IDES

Bexloy® V-572

Thermoplastic Elastomer

Supplied by DuPont Packaging & Industrial Polymers

The technical datasheet with complete property values for Bexloy® V-572 is available to members of the Prospector Plastics Database.
Register to view full datasheet.
Register to View Full Datasheet
General  
Material Status 
  • Commercial: Discontinued
Availability 
  • Europe
  • North America
 
Features 
  • Good Surface Finish
  • Low Temperature Toughness
  • Paintable
Uses 
  • Automotive Exterior Parts
Automotive Specifications 
Appearance 
  • Black
  • Grey
  • Red
  • White
 
Forms 
  • Pellets
Processing Method 
  • Injection Molding
Physical
Nominal Value
Unit
Test Method
Specific Gravity
 
ASTM D792
Melt Mass-Flow Rate (MFR) (240°C/2.16 kg)
g/10 min
ASTM D1238
Molding Shrinkage
    ASTM D955
Flow
in/in
 
Across Flow
in/in
 
Water Absorption (24 hr)
%
ASTM D570
Mechanical
Nominal Value
Unit
Test Method
Tensile Strength
    ASTM D638
Yield, 73°F
psi
 
73°F
psi
 
Tensile Elongation
    ASTM D638
Yield, 73°F
%
 
Break, 73°F
%
 
Flexural Modulus
    ASTM D790
-22°F
psi
 
73°F
psi
 
158°F
psi
 
Taber Abrasion Resistance (1000 Cycles, 1000 g, CS-17 Wheel)
mg
ASTM D1044
Elastomers
Nominal Value
Unit
Test Method
Tear Strength 2
lbf/in
ASTM D624
Impact
Nominal Value
Unit
Test Method
Notched Izod Impact
    ASTM D256
-22°F
ft·lb/in
 
73°F
ft·lb/in
 
Gardner Impact 3 (-22°F)
in·lb
ASTM D3029
Hardness
Nominal Value
Unit
Test Method
Durometer Hardness (Shore D)
 
ASTM D2240
Thermal
Nominal Value
Unit
Test Method
Deflection Temperature Under Load
    ASTM D648
66 psi, Unannealed
°F
 
264 psi, Unannealed
°F
 
Melting Temperature
°F
 
CLTE
    ASTM E831
Flow: -22 to 73°F
in/in/°F
 
Flow: 73 to 180°F
in/in/°F
 
Transverse: -22 to 73°F
in/in/°F
 
Transverse: 73 to 180°F
in/in/°F
 
Specific Heat
Btu/lb/°F
ASTM C351
Additional Information
The value for Melting Point was tested in accordance with ASTM D3418.
Heat Sag, ASTM D3769, 152mm (6in) overhang, 60 min, @ 250°F: 0.3 in
Heat of Fusion: 9.0 BTU/lb
Rheometric Impact, ultimate energy, 5mph, 1/2in dia. Tup, -22°F: 40 in-lb
Rheometric Impact, ultimate force, 5mph, 1/2in dia. Tup, -22°F: 360 lb
Melt Viscosity, Kayeness, 1000 s-1 shear rate, 464°F: 200 Pa-s
Specific Volume, ASTM D792: 19 in³/lb
Specific Heat, DSC, 122°F: 0.35 BTU/lb/°F
Specific Heat, DSC, 212°F: 0.38 BTU/lb/°F
Specific Heat, DSC, 302°F: 0.43 BTU/lb/°F
Specific Heat, DSC, 482°F: 0.51 BTU/lb/°F
Related Terminology
Product names can be difficult to match. You may have searched any one of these terms to find this product: Bexloy® V-572, Bexloy V572, Bexloy® , Bexloy, BexloyV572, V-572, V572, V:572, V/572, V+572, V_572, V 572, Thermoplastic Elastomer, TPE, DuPont P&IP, ThermoplasticElastomer, 572V
Features
Features may also be described by the following terms: Good Surface Finish, Low Temperature Toughness.
Automotive Specifications
This plastic material has approval for 1 automotive specifications from the following agencies (the number in parentheses shows the number of specifications for that agency): GM (1).
Injection
Nominal Value
Unit
 
Rear Temperature
°F
 
Middle Temperature
°F
 
Front Temperature
°F
 
Nozzle Temperature
°F
 
Processing (Melt) Temp
°F
 
Mold Temperature
°F
 
Injection Pressure
psi
 
Notes
1Typical properties: these are not to be construed as specifications.
2Die C
3Method G, Geometry GB
 
IDES
Copyright © 2012 IDES
The information presented on this datasheet was acquired by IDES from the producer of the material. IDES makes substantial efforts to assure the accuracy of this data. However, IDES assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.