The value for Melting Point was tested in accordance with ASTM D3418. Heat Sag, ASTM D3769, 152mm (6in) overhang, 60 min, @ 250°F: 0.5 in Heat of Fusion: 8.5 BTU/lb Rheometric Impact, ultimate energy, 5mph, 1/2in dia. Tup, -22°F: 150 in-lb Rheometric Impact, ultimate force, 5mph, 1/2in dia. Tup, -22°F: 540 lb Melt Viscosity, Kayeness, 1000 s-1 shear rate, 464°F: 240 Pa-s Specific Volume, ASTM D792: 23 in³/lb Specific Heat, DSC, 122°F: 0.38 BTU/lb/°F Specific Heat, DSC, 212°F: 0.41 BTU/lb/°F Specific Heat, DSC, 302°F: 0.46 BTU/lb/°F Specific Heat, DSC, 482°F: 0.61 BTU/lb/°F
|
|