Compression Set, ASTM D395, 22 hr, 302°F, Specimen post-cured 1 hr at 302°F: 20% Compression Set, ASTM D395, 22 hr, 302°F, Specimen post-cured 4 hrs at 392°F: 6% Viscosity, Part A: 480 Pa.s Viscosity, Part B: 480 Pa.s Cure Rate, ODR, 302°F, T10: 44 sec Cure Rate, ODR, 302°F, T90: 63 sec Press Cure, 5 min at 248°F
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: Shincor LIM KE1950-40, Shincor LIM KE195040, Shincor LIM , ShincorLIMKE195040, ShincorLIM, KE 1950, LIMKE 1950 40, LIMKE 1950, LIMKE1950-40, LIMKE195040, LIMKE1950:40, LIMKE1950/40, LIMKE1950+40, LIMKE1950_40, LIMKE1950 40, LIMKE1950, KE 1950 40, KE1950-40, KE195040, KE1950:40, KE1950/40, KE1950+40, KE1950_40, KE1950 40, KE1950, 195040, Silicone, Shincor Sil, 1950KE, 1950LIMKE
|