Texin® 260

Thermoplastic Polyurethane Elastomer (Polyester)

Supplied by Bayer MaterialScience LLC

The technical datasheet with complete property values for Texin® 260 is available to members of the Prospector Plastics Database.
Register to view full datasheet.
Register to View Full Datasheet
Product Description
Aromatic polyester-based thermoplastic polyurethane with Shore D hardness of approximately 60 for injection molding. Extrusion not recommended.
General  
Material Status 
  • Commercial: Active
Availability 
  • North America
Features 
  • Aromatic
Agency Ratings 
RoHS Compliance 
Processing Method 
  • Injection Molding
Multi-Point Data 
  • Shear Modulus vs. Temperature (ISO 11403-1)
Physical
Nominal Value
Unit
Test Method
Specific Gravity
     
--
 
ASTM D792
--
lb/in³
ISO 1183 2
Molding Shrinkage
    ASTM D955
Flow
in/in
 
Across Flow
in/in
 
Mechanical
Nominal Value
Unit
Test Method
Tensile Stress (50% Strain)
psi
ISO 527-2 2
Tensile Strain (Break)
%
ISO 527-2 2
Flexural Modulus (73°F)
psi
ASTM D790
Taber Abrasion Resistance (73°F, 1000 Cycles, 1000 g, H-18 Wheel)
mg
ASTM D1044
Elastomers
Nominal Value
Unit
Test Method
Tensile Stress
    ASTM D412
50% Strain, 73°F
psi
 
100% Strain, 73°F
psi
 
300% Strain, 73°F
psi
 
Tensile Strength (Break, 73°F)
psi
ASTM D412
Tensile Elongation (Break, 73°F)
%
ASTM D412
Tear Strength 3 (73°F)
lbf/in
ASTM D624
Compression Set
    ASTM D395B
73°F, 22.0 hr 4
%
 
73°F, 22.0 hr
%
 
158°F, 22.0 hr 4
%
 
158°F, 22.0 hr
%
 
Bayshore Resilience
%
ASTM D2632
Hardness
Nominal Value
Unit
Test Method
Durometer Hardness (Shore D, 73°F)
 
ASTM D2240
Thermal
Nominal Value
Unit
Test Method
Deflection Temperature Under Load
     
66 psi, Unannealed
°F
ASTM D648
66 psi
°F
ISO 75-2 2
Brittleness Temperature
°F
ASTM D746
Glass Transition Temperature
     
--
°F
DMA
-- 5
°F
ISO 11357-2 2
Vicat Softening Temperature
     
--
°F
ASTM D1525 6
50°C/h, B (50N)
°F
ISO 306 2
CLTE
     
Flow
in/in/°F
ASTM D696
Flow
in/in/°F
ISO 11359-2 2
Transverse
in/in/°F
ASTM D696
Flammability
Nominal Value
Unit
Test Method
Burning Behav. at 1.6mm nom. thickn. (0.06 in, UL)
 
ISO 1210 2
Additional Information
Nominal Value
Unit
Test Method
Compressive Load
    ASTM D575
73°F 7
psi
 
73°F 8
psi
 
73°F 9
psi
 
73°F 10
psi
 
73°F 11
psi
 
73°F 12
psi
 
73°F 13
psi
 
Related Terminology
Product names can be difficult to match. You may have searched any one of these terms to find this product: Texin® 260, Texin 260, Texin® , Texin, Texin260, 260, Thermoplastic Polyurethane Elastomer, Thermoplastic Polyurethane Elastomer (Polyester), Thermoplastic Polyurethane Elastomer Polyester, TPU-Polyester, TPUPolyester, TPU:Polyester, TPU/Polyester, TPU+Polyester, TPU_Polyester, TPU Polyester, Thermoplastic Polyurethane, TPU, Bayer, ThermoplasticPolyurethaneElastomerPolyester, ThermoplasticPolyurethane
Agency Ratings
This plastic material has 5 certifications from the following agencies (the number in parentheses shows the number of certifications for that agency): EU (3), FDA (2).
Notes
1Typical properties: these are not to be construed as specifications.
2Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted.
3Die C
4Post Cured for 16 hr at 230°F
518 °F/min
6Rate A (50°C/h), Loading 1 (10 N)
720% Deflection
825% Deflection
950% Deflection
1015% Deflection
112% Deflection
125% Deflection
1310% Deflection
 
IDES
Copyright © 2012 IDES
The information presented on this datasheet was acquired by IDES from the producer of the material. IDES makes substantial efforts to assure the accuracy of this data. However, IDES assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.