Ball Indentation Hardness, ISO 2039, Surface as Molded: 213 to 217 MPa Ball Indentation Hardness, ISO 2039, Polished Surface: 139 to 143 MPa
Flexural Strain @ Break, ISO 178, -30°C: 1.9 to 2.3% Flexural Strain @ Break, ISO 178, 23°C: 1.4 to 2.4% Flexural Strain @ Break, ISO 178, 100°C: 1.6 to 2.2% Flexural Strain @ Break, ISO 178, 200°C: 1.5 to 1.7% Flexural Strain @ Break, ISO 178, 300°C: 2.5 to 3.1%
CLTE, Test Method Unspecified, 212 to 392°F (100 to 200°C): 2.6 E-5 in/in/°F CLTE, Test Method Unspecified, 392 to 572°F (200 to 300°C): 2.5 E-5 in/in/°F CLTE, Test Method Unspecified, 572 to 680°F (300 to 360°C): 2.2 E-5 in/in/°F
|
|