Density
|
|
g/cm³
|
ISO 1183 |
|
Melt Mass-Flow Rate (MFR) (220°C/10.0 kg)
|
|
g/10 min
|
ISO 1133 |
|
Melt Volume-Flow Rate (MVR) (220°C/10.0 kg)
|
|
in³/10min
|
ISO 1133 |
|
Molding Shrinkage - Flow 2
|
|
in/in
|
Internal Method |
|
Water Absorption
|
|
|
ISO 62 |
|
Saturation, 73°F
|
|
%
|
|
|
Equilibrium, 73°F, 50% RH
|
|
%
|
|
|
Tensile Modulus
|
|
psi
|
ISO 527-2/1 |
|
Tensile Stress
|
|
|
|
|
Yield
|
|
psi
|
ISO 527-2/5 |
|
Yield
|
|
psi
|
ISO 527-2/50 |
|
Break
|
|
psi
|
ISO 527-2/5, ISO 527-2/50 |
|
Tensile Strain
|
|
|
|
|
Yield
|
|
%
|
ISO 527-2/5, ISO 527-2/50 |
|
Break
|
|
%
|
ISO 527-2/5 |
|
Break
|
|
%
|
ISO 527-2/50 |
|
Flexural Modulus 3
|
|
psi
|
ISO 178 |
|
Flexural Strength 3, 4
|
|
psi
|
ISO 178 |
|
Taber Abrasion Resistance (1000 Cycles, 1000 g, CS-17 Wheel)
|
|
mg
|
Internal Method |
|
Charpy Notched Impact Strength 5
|
|
|
ISO 179/1eA |
|
-22°F
|
|
ft·lb/in²
|
|
|
73°F
|
|
ft·lb/in²
|
|
|
Notched Izod Impact Strength 6
|
|
|
ISO 180/1A |
|
-22°F
|
|
ft·lb/in²
|
|
|
73°F
|
|
ft·lb/in²
|
|
|
Rockwell Hardness (R-Scale)
|
|
|
ISO 2039-2 |
|
Ball Indentation Hardness (H 358/30)
|
|
psi
|
ISO 2039-1 |
|
Heat Deflection Temperature 7
|
|
|
|
|
66 psi, Unannealed, 3.94 in Span
|
|
°F
|
ISO 75-2/Be |
|
264 psi, Unannealed, 3.94 in Span
|
|
°F
|
ISO 75-2/Ae |
|
Vicat Softening Temperature
|
|
|
|
|
--
|
|
°F
|
ISO 306/B50 |
|
--
|
|
°F
|
ISO 306/B120 |
|
Ball Pressure Test (167°F)
|
|
|
IEC 60695-10-2 |
|
CLTE
|
|
|
ISO 11359-2 |
|
Flow: 73 to 140°F
|
|
in/in/°F
|
|
|
Transverse: 73 to 140°F
|
|
in/in/°F
|
|
|
Thermal Conductivity
|
|
Btu·in/hr/ft²/°F
|
ISO 8302 |
|
Surface Resistivity
|
|
ohms
|
IEC 60093 |
|
Volume Resistivity
|
|
ohm·cm
|
IEC 60093 |
|
Relative Permittivity
|
|
|
IEC 60250 |
|
50 Hz
|
|
|
|
|
60 Hz
|
|
|
|
|
1 MHz
|
|
|
|
|
Dissipation Factor
|
|
|
IEC 60250 |
|
50 Hz
|
|
|
|
|
60 Hz
|
|
|
|
|
1 MHz
|
|
|
|
|
Comparative Tracking Index
|
|
V
|
IEC 60112 |
|
Electric Strength
|
|
|
IEC 60243-1 |
|
0.0315 in, in Oil
|
|
V/mil
|
|
|
0.0630 in, in Oil
|
|
V/mil
|
|
|
0.126 in, in Oil
|
|
V/mil
|
|
|
Flame Rating - UL
|
|
|
UL 94 |
|
0.0591 in
|
|
|
|
|
0.118 in
|
|
|
|
|
Glow Wire Flammability Index (0.0394 in)
|
|
°F
|
IEC 60695-2-12 |
|
RTI Str
|
|
°F
|
UL 746 |
|
RTI Imp
|
|
°F
|
UL 746 |
|
RTI Elec
|
|
°F
|
UL 746 |
|
This supplier and product may also be known by these terms: GE Plastics Europe, LNP Engineering Plastics, GE Polymerland Europe, GE Polymerland, GE Plastics, Cyclac
Product names can be difficult to match. You may have searched any one of these terms to find this product: CYCOLAC* GPM5500S Resin, CYCOLAC GPM5500S Resin, CYCOLAC* , CYCOLAC, CYCOLACGPM5500SResin, GPM 5500 S Resin, GPM5500S Resin, GPM5500, 5500S, SResin, GPM5500SResin, Acrylonitrile Butadiene Styrene, ABS, SABIC IP Euro, AcrylonitrileButadieneStyrene, 5500GPM
|
|
Features may also be described by the following terms: Good Processability, Easy Processing.
|
|
Uses may also be described by the following terms: Appliance Components, Appliance Parts, Business Equipment, Business Machines.
|