Spiral Flow, SB-U-03-003: 100 cm Gel Time, SB-U-03-005, 175°C: 25 sec
Thermal Expansion, SB-U-02-002, T<Tg: 1.0 E-5/°C Thermal Expansion, SB-U-02-002, T>Tg: 4.2 E-5/°C
Flexural Strength, SB-U-01-001, 240°C: 21.6 MPa Flexural Modulus, SB-U-01-002, 240°C: 736 MPa
UL-94 Flame Class, SB-U-03-003: V-0
Extracted Na+, SB-U-04-043: <1 ppm Extracted Cl-, SB-U-04-043: 5 ppm
Transfer Pressure: 687-1177 MPa
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: Sumikon® EME-7351LS, Sumikon EME7351LS, Sumikon® , Sumikon, SumikonEME7351LS, EME, EME 7351 LS, EME-7351LS, EME7351LS, EME:7351LS, EME/7351LS, EME+7351LS, EME_7351LS, EME 7351LS, EME7351, 7351LS, Epoxy; Epoxide, Epoxy Epoxide, Epoxy, Sumitomo Bake, EpoxyEpoxide, 7351EME
|