Spiral Flow, SB-U-03-003: 80 cm Gel Time, SB-U-03-005, 175°C: 30 sec Thermal Expansion, SB-U-02-002, T<Tg: 1.3 E-5/°C Thermal Expansion, SB-U-02-002, T>Tg: 4.1 E-5/°C Flexural Strength, SB-U-01-001, 240°C: 44.1 MPa Flexural Modulus, SB-U-01-002, 240°C: 2650 MPa UL-94 Flame Class, SB-U-03-003: V-0 Extracted Na+, SB-U-04-043: <1 ppm Extracted Cl-, SB-U-04-043: 5 ppm Transfer Pressure: 687-1177 MPa
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: Sumikon® EME-7720R, Sumikon EME7720R, Sumikon® , Sumikon, SumikonEME7720R, EME, EME 7720 R, EME-7720R, EME7720R, EME:7720R, EME/7720R, EME+7720R, EME_7720R, EME 7720R, EME7720, 7720R, Epoxy; Epoxide, Epoxy Epoxide, Epoxy, Sumitomo Bake, EpoxyEpoxide, 7720EME
|