Density, ASTM D 792: 1.35-1.37. Water Absorption 24h, ASTM D 570: 0.5-0.7%. The value listed as C.T.I., UL 746: >550, was tested in accordance with CEI 112. GWI, 850°C 1.6 mm, NO.
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: Sebimid 66 66 G6 HS, Sebimid 66 , Sebimid6666G6HS, Sebimid66, 6666 G 6 HS, 6666 G6 HS, 6666G, 66, 66 G 6 HS, 6666G6HS, 66 G6 HS, 66G, G6, 6HS, 66G6HS, Polyamide 6, Nylon 6, Polyamide, Nylon, pa6, Sebi, Polyamide6, Nylon6, G66, G6666
|
|
Features may also be described by the following terms: Heat Stabilized, Heat-ageing Stabilized, Heat Ageing Stabilized, Heat-aging Stabilized, Heat Aging Stabilized.
|