The value listed as Unnotched Izod Impact, ASTM D256, was tested in accordance with ASTM D4812. Filler Content, ASTM D2584: 40.0% Testing and measurements were performed at 73 +/-3°F and 50 +/-5% relative humidity unless otherwise noted.
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: GAPEX® APP40GR17HB-NA, GAPEX APP40GR17HBNA, GAPEX® , GAPEX, GAPEXAPP40GR17HBNA, APP 40 GR 17 HB, APP40GR17HB, APP 40 GR 17 HB NA, APP40GR17HB-NA, APP40GR17HBNA, APP40GR17HB:NA, APP40GR17HB/NA, APP40GR17HB+NA, APP40GR17HB_NA, APP40GR17HB NA, APP40, 40GR, GR17, 17HB, HBNA, Polypropylene Homopolymer, PP Homopolymer, Polypropylene, PP, Ferro, PolypropyleneHomopolymer, PPHomopolymer, 40APP
|
|
Features may also be described by the following terms: Heat Stabilized, Heat-ageing Stabilized, Heat Ageing Stabilized, Heat-aging Stabilized, Heat Aging Stabilized.
|