0.157 in, Energy to Peak Force
|
|
ft·lb
|
|
|
0.157 in, Total Penetration Energy
|
|
ft·lb
|
|
|
Mass Per Unit Area, Azdel Test Method: 4.500 kg/m² Thickness, Azdel Test Method: 4.4 mm Density, ISO 1183 Test Method: 1.02 g/cm³ Density, ISO 1183 Test Method, Molded Plaque: 1.06 g/cm³ Recrystallizing Temperature, ISO 3146 Test Method: 115 °C CTLE, Azdel Test Method, -30°C to 0°C, 3mm: 5.2e-5 1/°C CTLE, Azdel Test Method, 0°C to 120°C, 3mm: 3.8e-5 1/°C Blank Heat Parameters -Internal Temperature: 190 to 215°C -Surface Temperature: 205 to 220°C -Typical Heating Time for IR-System: 180 to 240°C -Typical Heating Time for Hot Air System: 240 to 480°C Mould Temperature: 30 to 90°C Moulding Preasure: 150 to 250 bar Minimum Pressing Speed: 20 mm/sec Total Cycle Time: 30 to 90 sec
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: AZDEL* C200B01N, AZDEL C200B01N, AZDEL* , AZDEL, AZDELC200B01N, C 200 B 01 N, C200B01N, C200, 200B, B01, 01N, Polypropylene Alloy, PP Alloy, Polypropylene, PP, PolypropyleneAlloy, PPAlloy, 200C
|