0.157 in, Energy to Peak Force
|
|
ft·lb
|
|
|
0.157 in, Total Penetration Energy
|
|
ft·lb
|
|
|
Mass Per Unit Area, Azdel Test Method: 4.840 kg/m² Thickness, Azdel Test Method: 3.9 mm Density, ISO 1183 Test Method: 1.21 g/cm³ Density, ISO 1183 Test Method, Molded Plaque: 1.25 g/cm³ Recrystallizing Temperature, ISO 3146 Test Method: 119 °C CTLE, Azdel Test Method, -30°C to 0°C, 3mm: 5.0e-5 1/°C CTLE, Azdel Test Method, 0°C to 120°C, 3mm: 3.3e-5 1/°C Blank Heat Parameters -Internal Temperature: 190 to 215°C -Surface Temperature: 205 to 220°C -Typical Heating Time for IR-System: 180 to 240°C -Typical Heating Time for Hot Air System: 240 to 480°C Mould Temperature: 30 to 90°C Moulding Preasure: 150 to 250 bar Minimum Pressing Speed: 20 mm/sec Total Cycle Time: 30 to 90 sec
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: AZDEL* U421B02N, AZDEL U421B02N, AZDEL* U421B02N (Transverse), AZDEL U421B02N Transverse, AZDEL* , AZDEL, AZDELU421B02NTransverse, U 421 B 02 N, U421B02N, U 421 B 02 N Transverse, U421B02N (Transverse), U421B02N Transverse, U421, 421B, B02, 02N, NTransverse, U421B02NTransverse, Polypropylene Alloy, PP Alloy, Polypropylene, PP, PolypropyleneAlloy, PPAlloy, 421U
|