IDES Prospector Already have an account? Login Here

IDES

TAROBLEND 65

Acrylonitrile Butadiene Styrene + PC

Supplied by Taro Plast S.p.A.

The technical datasheet with complete property values for TAROBLEND 65 is available to members of the Prospector Plastics Database.
Register to view full datasheet.
Register to View Full Datasheet
Product Description
PC/ABS alloy medium-high thermal resistance, good flow and mechanical properties, low moisture absorption and good dimensional stability.

FIAT CR 110.500 - FORD TL 522 31 (Type B)

Available: all colors, UV stabilized (L).
General  
Material Status 
  • Commercial: Active
Availability 
  • Europe
Additive 
  • UV Stabilizer
Features 
  • Good Dimensional Stability
  • Good Flow
  • Good UV Resistance
  • Low Moisture Absorption
  • Medium Heat Resistance
Appearance 
  • Colors Available
Forms 
  • Pellets
Processing Method 
  • Injection Molding
Physical
Nominal Value
Unit
Test Method
Specific Gravity
     
--
 
ASTM D792
--
g/cm³
ISO 1183
Melt Mass-Flow Rate (MFR) (260°C/5.0 kg)
g/10 min
ASTM D1238, ISO 1133
Molding Shrinkage
    ASTM D955
Flow
in/in
 
Across Flow
in/in
 
Water Absorption
    ASTM D570, ISO 62
73°F, 24 hr
%
 
Saturation, 73°F
%
 
Mechanical
Nominal Value
Unit
Test Method
Tensile Modulus
psi
ASTM D638, ISO 527-2
Tensile Strength (Yield)
psi
ASTM D638, ISO 527-2
Tensile Elongation (Break)
%
ASTM D638, ISO 527-2
Flexural Modulus
psi
ASTM D790, ISO 178
Flexural Strength
     
--
psi
ISO 178
Break
psi
ASTM D790
Impact
Nominal Value
Unit
Test Method
Charpy Notched Impact Strength 2 (73°F)
ft·lb/in²
ASTM D256, ISO 179
Charpy Unnotched Impact Strength 2 (73°F)
 
ASTM D256, ISO 179
Notched Izod Impact (73°F, 0.126 in)
ft·lb/in
ISO 180, ASTM D256
Thermal
Nominal Value
Unit
Test Method
Deflection Temperature Under Load (264 psi, Unannealed)
°F
ASTM D648, ISO 75-2/A
Max. Continuous Use Temperature 3
°F
IEC 60216
Vicat Softening Temperature
     
--
°F
ASTM D1525 4, ISO 306/A50 4
--
°F
ASTM D1525 5, ISO 306/B50 5
Ball Pressure Test (257°F)
 
VDE 0470
CLTE - Flow (-22 to 86°F)
in/in/°F
ASTM D696
Electrical
Nominal Value
Unit
Test Method
Volume Resistivity
ohm·cm
ASTM D257
Dielectric Strength (0.0787 in)
V/mil
ASTM D149
Comparative Tracking Index (Solution A)
V
IEC 60112
Flammability
Nominal Value
Unit
Test Method
Burning Rate
in/min
FMVSS 302
Flame Rating - UL (0.0630 in)
 
UL 94
Oxygen Index
%
ASTM D2863
Related Terminology
Product names can be difficult to match. You may have searched any one of these terms to find this product: TAROBLEND 65, TAROBLEND , TAROBLEND65, 65, Acrylonitrile Butadiene Styrene + PC, Acrylonitrile Butadiene Styrene PC, Acrylonitrile Butadiene Styrene : PC, Acrylonitrile Butadiene Styrene / PC, Acrylonitrile Butadiene Styrene - PC, Acrylonitrile Butadiene Styrene _ PC, Acrylonitrile Butadiene Styrene PC, ABS+PC, ABSPC, ABS:PC, ABS/PC, ABS-PC, ABS_PC, ABS PC, Acrylonitrile Butadiene Styrene, ABS, Taro Plast, AcrylonitrileButadieneStyrenePC, AcrylonitrileButadieneStyrene, AcrylonitrileButadieneStyrene_PC
Features
Features may also be described by the following terms: Good Flow, Low Moisture Absorption, Low Water Absorption, Water Resistant, Moisture Resistant, Good Dimensional Stability, Dimensionally Stable, Medium Heat Resistance, Good UV Resistance, UV Resistant, Ultraviolet Resistant, Ultraviolet Light Resistant.
Injection
Nominal Value
Unit
 
Drying Temperature
     
--
°F
 
Pre-heater
°F
 
Drying Time
     
--
hr
 
Pre-heater
hr
 
Processing (Melt) Temp
°F
 
Mold Temperature
°F
 
Injection Rate
 
 
Notes
1Typical properties: these are not to be construed as specifications.
26x4x50 mm
320000 hrs
4Rate A (50°C/h), Loading 1 (10 N)
5Rate A (50°C/h), Loading 2 (50 N)
 
IDES
Copyright © 2012 IDES
The information presented on this datasheet was acquired by IDES from the producer of the material. IDES makes substantial efforts to assure the accuracy of this data. However, IDES assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.