Tests were performed in accordance with JIS K6911 Flexural Strength, JIS K6911, Flow: 150 Mpa Flexural Strength, JIS K6911, Accross Flow: 130 Mpa Solvent Resistivity, JIS K6911, 30 min boil: Constant Dielectric Strength, JIS K6911, Flatwise: 20 MV/m Punching Shrinkage, JIS K6911, 60°C, 150 mm length, Flow: 0.13% Punching Shrinkage, JIS K6911, 60°C, 150 mm length, Across Flow: 0.22% Punching Temperature, JIS K6911: 90°C Insulation Resistance, JIS K6911: 5e4 M ohms Insulation Resistance JIS K6911: 5e1 M ohms Heat Resistivity, JIS K6911, 120 min: 120°C
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: SUMILITE® PL-1252, SUMILITE PL 1252, SUMILITE® PL-1252 (Punching), SUMILITE PL1252 Punching, SUMILITE® , SUMILITE, SUMILITEPL1252Punching, PL, PL-1252, PL 1252, PL-1252 (Punching), PL1252 Punching, PL:1252 (Punching), PL:1252, PL/1252 (Punching), PL/1252, PL+1252 (Punching), PL+1252, PL_1252 (Punching), PL_1252, PL 1252 (Punching), PL1252, 1252Punching, PL1252Punching, PL_1252 Punching, PL 1252 Punching, PL_1252Punching, Phenolic, Sumitomo Bake, 1252PL
|