Density
|
|
g/cm³
|
ISO 1183 |
|
Tensile Stress - Across Flow 2
|
|
|
ISO 37 |
|
100% Strain
|
|
psi
|
|
|
300% Strain
|
|
psi
|
|
|
Tensile Stress - Across Flow 2 (Break)
|
|
psi
|
ISO 37 |
|
Tensile Elongation - Across Flow 2 (Break)
|
|
%
|
ISO 37 |
|
Compression Set (158°F, 22.0 hr)
|
|
%
|
ISO 815 |
|
Shore Hardness
|
|
|
ISO 868 |
|
Shore A, 5 sec, Injection Molded
|
|
|
|
|
Shore D, 5 sec, Injection Molded
|
|
|
|
|
Change in Tensile Strength in Air
|
|
|
ISO 188 |
|
257°F, 672 hr
|
|
%
|
|
|
302°F, 336 hr
|
|
%
|
|
|
Change in Tensile Strain at Break in Air
|
|
|
ISO 188 |
|
257°F, 672 hr
|
|
%
|
|
|
302°F, 336 hr
|
|
%
|
|
|
Change in Shore Hardness in Air
|
|
|
ISO 188 |
|
Shore A, 257°F, 672 hr
|
|
|
|
|
Shore D, 302°F, 336 hr
|
|
|
|
|
Change in Volume
|
|
|
ISO 1817 |
|
73°F, 168 hr, in Reference Fuel B
|
|
%
|
|
|
212°F, 72 hr, in Water
|
|
%
|
|
|
212°F, 168 hr, in ASTM #1 Oil
|
|
%
|
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: Sarlink® 3790-40, Sarlink 379040, Sarlink® , Sarlink, Sarlink379040, 3790, 3790-40, 379040, 3790:40, 3790/40, 3790+40, 3790_40, 3790 40, Thermoplastic Vulcanizate, TPV, Thermoplastic Elastomer, TPE, ThermoplasticVulcanizate, ThermoplasticElastomer, 403790
|
|
Features may also be described by the following terms: High Hardness, Hard, High Flow, High Melt, High MFI, Good UV Resistance, UV Resistant, Ultraviolet Resistant, Ultraviolet Light Resistant, Good Surface Finish, Medium Heat Resistance.
|
|
Uses may also be described by the following terms: Automotive Applications, Automotive Sector.
|