Product Description
Developmental product
Polyether-based thermoplastic polyurethane with a Shore hardness of approximately 90A. It can be processed by injection molding or extrusion.
Application: Typical applications belting, hose, seals, gaskets, tubing, cable jackets, hose jackets, athletic shoe soles, casters, film, extruded profiles, and miscellaneous molded articles.
General  
Material Status 
  • Commercial: Active
Availability 
  • North America
Uses 
  • Belts/Belt Repair
  • Cable Jacketing
  • Film
  • Footwear
  • Gaskets
  • Hose
  • Profiles
  • Seals
  • Tubing
Agency Ratings 
RoHS Compliance 
Forms 
  • Pellets
Processing Method 
  • Extrusion
  • Injection Molding
 
Physical
Nominal Value
Unit
Test Method
Specific Gravity
 
ASTM D792
Molding Shrinkage
    ASTM D955
Flow
in/in
 
Across Flow
in/in
 
Mechanical
Nominal Value
Unit
Test Method
Flexural Modulus (73°F)
psi
ASTM D790
Taber Abrasion Resistance (1000 Cycles, 1000 g, H-18 Wheel)
mg
ASTM D1044
Elastomers
Nominal Value
Unit
Test Method
Tensile Stress
    ASTM D412
50% Strain
psi
 
100% Strain
psi
 
300% Strain
psi
 
Tensile Strength (Yield)
psi
ASTM D412
Tensile Elongation (Break)
%
ASTM D412
Tear Strength 2
lbf/in
ASTM D624
Compression Set
    ASTM D395B
73°F, 22.0 hr
%
 
158°F, 22.0 hr
%
 
Bayshore Resilience
%
ASTM D2632
Hardness
Nominal Value
Unit
Test Method
Durometer Hardness (Shore A)
 
ASTM D2240
Thermal
Nominal Value
Unit
Test Method
Brittleness Temperature
°F
ASTM D746
Vicat Softening Temperature
°F
ASTM D1525 3
Additional Information
Compression set, post-cured, ASTM D395-B, 22 h at 73 °F, post-cured 16 h at 230 °F: 13 %
Compression set, post-cured, ASTM D395-B, 22 h at 158 °F, post-cured 16 h at 230 °F: 35 %
Compressive load, ASTM D575, 2% deflection: 100 psi
Compressive load, ASTM D575, 5% deflection: 250 psi
Compressive load, ASTM D575, 10% deflection: 450 psi
Compressive load, ASTM D575, 15% deflection: 650 psi
Compressive load, ASTM D575, 20% deflection: 850 psi
Compressive load, ASTM D575, 25% deflection: 1050 psi
Compressive load, ASTM D575, 50% deflection: 2800 psi
Glass transition temperature, DMA, DMA: -47 °F
Related Terminology
Product names can be difficult to match. You may have searched any one of these terms to find this product: Texin® 1050, Texin 1050, Texin® , Texin, Texin1050, 1050, Thermoplastic Polyurethane Elastomer, Thermoplastic Polyurethane Elastomer (Polyether), Thermoplastic Polyurethane Elastomer Polyether, TPU-Polyether, TPUPolyether, TPU:Polyether, TPU/Polyether, TPU+Polyether, TPU_Polyether, TPU Polyether, Thermoplastic Polyurethane, TPU, Bayer, ThermoplasticPolyurethaneElastomerPolyether, ThermoplasticPolyurethane
Uses
Uses may also be described by the following terms: Gaskets, Gasketing, Belts/Belt Repair, Belt Repair, Tubing, Tube.
Agency Ratings
This plastic material has 3 certifications from the following agencies (the number in parentheses shows the number of certifications for that agency): EU (3).
Notes
1Typical properties: these are not to be construed as specifications.
2Die C
3Rate A (50°C/h), Loading 1 (10 N)
 
IDES
Copyright © 2012 IDES
The information presented on this datasheet was acquired by IDES from the producer of the material. IDES makes substantial efforts to assure the accuracy of this data. However, IDES assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.