IDES Prospector Already have an account? Login Here

IDES

Stanyl® TS256F8

Polyamide 46

Glass Fiber Reinforcement, 40%

Supplied by DSM Engineering Plastics

The technical datasheet with complete property values for Stanyl® TS256F8 is available to members of the Prospector Plastics Database.
Register to view full datasheet.
Register to View Full Datasheet
General  
Material Status 
  • Commercial: Active
Availability 
  • Asia Pacific
Filler / Reinforcement 
  • Glass Fiber Reinforcement, 40% Filler by Weight
Additive 
  • Flame Retardant
Features 
  • Flame Retardant
  • Low Moisture Absorption
 
RoHS Compliance 
Forms 
  • Pellets
Physical
Dry
Conditioned
Unit
Test Method
Density
--
g/cm³
ISO 1183
Water Absorption (Equilibrium, 73°F, 50% RH)
--
%
ISO 62
Mechanical
Dry
Conditioned
Unit
Test Method
Tensile Modulus
psi
ISO 527-2
Tensile Stress (Break)
psi
ISO 527-2
Tensile Strain (Break)
%
ISO 527-2
Impact
Dry
Conditioned
Unit
Test Method
Charpy Notched Impact Strength
      ISO 179/1eA
-22°F
ft·lb/in²
 
73°F
ft·lb/in²
 
Thermal
Dry
Conditioned
Unit
Test Method
Heat Deflection Temperature (264 psi, Unannealed)
--
°F
ISO 75-2/A
Melting Temperature 2
--
°F
ISO 11357-3
CLTE
      ISO 11359-2
Flow
--
in/in/°F
 
Transverse
--
in/in/°F
 
Flammability
Dry
Conditioned
Unit
Test Method
Flammability Classification
      IEC 60695-11-10, -20
0.0295 in
--
 
 
0.0591 in
--
 
 
Related Terminology
Dry
Product names can be difficult to match. You may have searched any one of these terms to find this product: Stanyl® TS256F8, Stanyl TS256F8, Stanyl® , Stanyl, StanylTS256F8, TS 256 F 8, TS256F8, TS256, 256F, F8, Polyamide 46, Nylon 46, Polyamide, Nylon, pa46, DSM EP, Polyamide46, Nylon46, 256TS
Generic Name
Dry
Generic Name may also be described by the following terms: PA46.
Conditioned
Generic Name may also be described by the following terms: PA46.
Features
Dry
Features may also be described by the following terms: Low Moisture Absorption, Low Water Absorption, Water Resistant, Moisture Resistant.
Conditioned
Product names can be difficult to match. You may have searched any one of these terms to find this product: Stanyl® TS256F8, Stanyl TS256F8, Stanyl® , Stanyl, StanylTS256F8, TS 256 F 8, TS256F8, TS256, 256F, F8, Polyamide 46, Nylon 46, Polyamide, Nylon, pa46, DSM EP, Polyamide46, Nylon46, 256TS
Injection
Dry
Unit
 
Suggested Max Moisture
%
 
Rear Temperature
°F
 
Middle Temperature
°F
 
Front Temperature
°F
 
Nozzle Temperature
°F
 
Processing (Melt) Temp
°F
 
Mold Temperature
°F
 
Injection Rate
 
 
Back Pressure
psi
 
Vent Depth
in
 
Notes
1Typical properties: these are not to be construed as specifications.
210°C/min
 
IDES
Copyright © 2012 IDES
The information presented on this datasheet was acquired by IDES from the producer of the material. IDES makes substantial efforts to assure the accuracy of this data. However, IDES assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.