IDES Prospector Already have an account? Login Here

IDES

Escor™ 5110 ExCo

Ethylene Acrylic Acid Copolymer Resin

Supplied by ExxonMobil Chemical

The technical datasheet with complete property values for Escor™ 5110 ExCo is available to members of the Prospector Plastics Database.
Register to view full datasheet.
Register to View Full Datasheet
Product Description
Escor 5110 is primarily intended for high speed, low coating weight extrusion coating and extrusion lamination.
Excellent adhesion to polar substrates, aluminum foil, polyamide films, metallized films, papers, iron, steel and glass. Very high bond resistance even for acidic and aggressive food products. Very low sealing and hot tack initiation temperature, very high hot tack peak force.
General  
Material Status 
  • Commercial: Active
Availability 
  • Africa & Middle East
  • Europe
 
Physical
Nominal Value
Unit
Test Method
Acrylic Acid Content
wt%
ExxonMobil Method
Thermal
Nominal Value
Unit
Test Method
Vicat Softening Temperature
°F
ASTM D1525
Legal Statement
Contact your ExxonMobil Chemical Customer Service Representative for potential food contact application compliance (e.g. FDA, EU, HPFB).

This product is not intended for use in medical applications and should not be used in any such applications.
Related Terminology
This supplier and product may also be known by these terms: Exxon, Exxon Mobil, Exxon Mobile, Advanced Elastomer Systems, AES

Product names can be difficult to match. You may have searched any one of these terms to find this product: Escor™ 5110 ExCo, Escor 5110 ExCo, Escor™ , Escor, Escor5110ExCo, 5110 ExCo, 5110ExCo, Ethylene Acrylic Acid Copolymer, EAA, Thermoplastic Elastomer, TPE, ExxonMobil, EthyleneAcrylicAcidCopolymer, ThermoplasticElastomer, ExCo5110
Extrusion Notes
Excellent results are obtained in extrusion coating at 260 - 280°C (500 - 536°F) temperature range. Processing temperatures above 300°C (572°F) may cause resin degradation.
To minimise corrosion risk, all exposed metal surfaces in the extruder and die should be made from corrosion resistant metals or nickel/chrome plated. ESCOR should be fed into the extruder after LDPE of a similar or higher melt index. Machines should always be completely purged with LDPE or a suitable cleaning compound before shutdown.
Notes
1Typical properties: these are not to be construed as specifications.
 
IDES
Copyright © 2012 IDES
The information presented on this datasheet was acquired by IDES from the producer of the material. IDES makes substantial efforts to assure the accuracy of this data. However, IDES assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.