Product Description
Escor 6000 is primarily intended for extrusion coating and coextrusion coating. Escor 6000 is the high draw down version of Escor 5000. Very low coating weight achievable at high line speed.
Very good adhesion to polar substrates, aluminum foil, metallized films, papers, iron, steel and glass. Offers excellent balance of adhesion onto the substrates and interlayer adhesion with coextruded LDPE and EVA's.
General  
Material Status 
  • Commercial: Active
Availability 
  • Africa & Middle East
  • Europe
 
Physical
Nominal Value
Unit
Test Method
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg)
g/10 min
ASTM D1238
Acrylic Acid Content
wt%
ExxonMobil Method
Legal Statement
Contact your ExxonMobil Chemical Customer Service Representative for potential food contact application compliance (e.g. FDA, EU, HPFB).

This product is not intended for use in medical applications and should not be used in any such applications.
Related Terminology
This supplier and product may also be known by these terms: Exxon, Exxon Mobil, Exxon Mobile, Advanced Elastomer Systems, AES

Product names can be difficult to match. You may have searched any one of these terms to find this product: Escor™ 6000 ExCo, Escor 6000 ExCo, Escor™ , Escor, Escor6000ExCo, 6000 ExCo, 6000ExCo, Ethylene Acrylic Acid Copolymer, EAA, Thermoplastic Elastomer, TPE, ExxonMobil, EthyleneAcrylicAcidCopolymer, ThermoplasticElastomer, ExCo6000
Extrusion Notes
Excellent results are obtained in extrusion coating at 260 - 280°C (500 - 536F) temperature range. Processing temperatures above 300°C (572°F) may cause resin degradation.
To minimise corrosion risk, all exposed metal surfaces in the extruder and die should be made from corrosion resistant metals or nickel/chrome plated. ESCOR should be fed into the extruder after LDPE of a similar or higher melt index. Machines should always be completely purged with LDPE or a suitable cleaning compound before shutdown.
Notes
1Typical properties: these are not to be construed as specifications.
 
IDES
Copyright © 2012 IDES
The information presented on this datasheet was acquired by IDES from the producer of the material. IDES makes substantial efforts to assure the accuracy of this data. However, IDES assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.