Compression Set, ASTM D395, 22 hr, 302°F, Specimen post-cured 1 hr at 302°F: 30% Compression Set, ASTM D395, 22 hr, 302°F, Specimen post-cured 4 hrs at 392°F: 5% Viscosity, Part A: 400 Pa.s Viscosity, Part B: 400 Pa.s Cure Rate, ODR, 302°F, T10: 20 sec Cure Rate, ODR, 302°F, T90: 29 sec Press Cure, 5 min at 248°F
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: Shincor LIM KE2001-40, Shincor LIM KE200140, Shincor LIM , ShincorLIMKE200140, ShincorLIM, KE 2001, LIMKE 2001 40, LIMKE 2001, LIMKE2001-40, LIMKE200140, LIMKE2001:40, LIMKE2001/40, LIMKE2001+40, LIMKE2001_40, LIMKE2001 40, LIMKE2001, KE 2001 40, KE2001-40, KE200140, KE2001:40, KE2001/40, KE2001+40, KE2001_40, KE2001 40, KE2001, 200140, Silicone, Shincor Sil, 2001KE, 2001LIMKE
|