HCI Generation: <4% Durometer Hardness, ASTM D2240, shore D, 20°C: 60 Hot Set Test, reading after 15, IEC 540, 20 N/cm² at 200°C: 30% Hot Set Test, residual value, IEC 540, 20 N/cm² at 200°C: 0% Crosslinking of the finished product is obtained by:
- Immersion of the bobbin in hot water at 85/90°C for two hours up to 3 mm thickness
- Steam treatment at 0.15 bar for 5/6 hours
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: GETILAN ATP/130-XH3A, GETILAN ATP130XH3A, GETILAN , GETILANATP130XH3A, ATP, ATP 130 XH 3 A, ATP/130-XH3A, ATP130XH3A, ATP:130-XH3A, ATP+130-XH3A, ATP-130-XH3A, ATP_130-XH3A, ATP 130-XH3A, ATP/130:XH3A, ATP/130/XH3A, ATP/130+XH3A, ATP/130_XH3A, ATP/130 XH3A, ATP130, 130XH, XH3, 3A, ATP_130XH3A, ATP 130XH3A, ATP130_XH3A, ATP130 XH3A, Polyethylene, Crosslinked, Polyethylene Crosslinked, XLPE, Polyethylene, PE, Crosspolimeri, PolyethyleneCrosslinked, 130ATP
|