IDES Prospector Already have an account? Login Here

IDES

GETILAN GPE/400

Crosslinked Polyethylene

Supplied by Crosspolimeri S.p.A.

The technical datasheet with complete property values for GETILAN GPE/400 is available to members of the Prospector Plastics Database.
Register to view full datasheet.
Register to View Full Datasheet
Product Description
GETILAN is our trade-mark of our crosslinkable polythene.
GETILAN GPE/400 is a medium density chemically crosslinkable compound for low voltage power cable insulation and sheathing.
It is a conveniently grafted polythene able to react in presence of moisture and of a catalyst. We normally suggest our catalyst type MAC/100 or MAC/202 red copper resistant.

REACTION BETWEEN GRAFTING AND CATALYST:
These two polythenes, separately stored, must be mixed before starting extrusion in the ratio:
GRAFTING/CATALYST 95/5
General  
Material Status 
  • Commercial: Active
Availability 
  • Europe
Features 
  • Crosslinkable
Uses 
  • Cable Jacketing
Agency Ratings 
Forms 
  • Pellets
Physical
Nominal Value
Unit
Test Method
Specific Gravity
 
ASTM D792
Melt Mass-Flow Rate (MFR) (190°C/5.0 kg)
g/10 min
ASTM D1238
Water Absorption - 24 hr (212°F)
lb/ream
IEC 60811
Mechanical
Nominal Value
Unit
Test Method
Tensile Stress (Yield)
psi
IEC 60811
Tensile Strain (Break)
%
IEC 60811
Thermal
Nominal Value
Unit
Test Method
Hot Set 2
    IEC 60811
392°F
%
 
Residual: 392°F
%
 
Aging
Nominal Value
Unit
Test Method
Change in Tensile Strength in Air
    IEC 60811
261°F, 40 hr
%
 
275°F, 168 hr
%
 
Change in Tensile Strain at Break in Air
    IEC 60811
261°F, 40 hr
%
 
275°F, 168 hr
%
 
Electrical
Nominal Value
Unit
Test Method
Volume Resistivity
ohm·cm
BS 6622
Related Terminology
Product names can be difficult to match. You may have searched any one of these terms to find this product: GETILAN GPE/400, GETILAN GPE400, GETILAN , GETILANGPE400, GPE, GPE/400, GPE400, GPE:400, GPE+400, GPE-400, GPE_400, GPE 400, Polyethylene, Crosslinked, Polyethylene Crosslinked, XLPE, Polyethylene, PE, Crosspolimeri, PolyethyleneCrosslinked, 400GPE
Agency Ratings
This plastic material has 1 certifications from the following agencies (the number in parentheses shows the number of certifications for that agency): IEC (1).
Extrusion
Nominal Value
Unit
 
Cylinder Zone 1 Temp.
°F
 
Cylinder Zone 2 Temp.
°F
 
Cylinder Zone 3 Temp.
°F
 
Cylinder Zone 4 Temp.
°F
 
Cylinder Zone 5 Temp.
°F
 
Die Temperature
°F
 
Extrusion Notes
CROSSLINKING:
Crosslinking of the finished product is obtained by:
  • Immersion of the bobbin into hot water at 85/90°C for some hours (up to 3 mm thickness).
  • Steam treatment at 0.15 for bar 5/6 hours.
  • Faster ambient curing is possible depending from the atmospheric conditions.
Notes
1Typical properties: these are not to be construed as specifications.
220 N/cm²
 
IDES
Copyright © 2012 IDES
The information presented on this datasheet was acquired by IDES from the producer of the material. IDES makes substantial efforts to assure the accuracy of this data. However, IDES assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.