Density
|
|
g/cm³
|
ISO 1183 |
|
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg)
|
|
g/10 min
|
ISO 1133 |
|
Molding Shrinkage (24 hr)
|
|
%
|
Internal Method |
|
Tensile Stress
|
|
|
ISO 527-2/5/50 |
|
Yield, 0.126 in, Injection Molded
|
|
psi
|
|
|
Break, 0.126 in, Injection Molded
|
|
psi
|
|
|
Tensile Strain (Break, 0.126 in, Injection Molded)
|
|
%
|
ISO 527-2/5/50 |
|
Flexural Modulus 2 (Injection Molded)
|
|
psi
|
ASTM D790 |
|
Charpy Notched Impact Strength (73°F, Injection Molded)
|
|
|
ISO 179/1eA |
|
Charpy Unnotched Impact Strength (-40°F, Injection Molded)
|
|
|
ISO 179/1eU |
|
Notched Izod Impact Strength
|
|
|
ISO 180/4A |
|
-4°F, Injection Molded
|
|
|
|
|
32°F, Injection Molded
|
|
|
|
|
73°F, Injection Molded
|
|
|
|
|
Shore Hardness (Shore D, Injection Molded)
|
|
|
ISO 868 |
|
Heat Deflection Temperature (66 psi, Unannealed)
|
|
°F
|
ISO 75-2/B |
|
CLTE - Flow
|
|
|
ASTM D696 |
|
-22 to 86°F
|
|
in/in/°F
|
|
|
73 to 176°F
|
|
in/in/°F
|
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: SABIC® PPcompound 8600, SABIC PPcompound 8600, SABIC® PPcompound , SABIC PPcompound, SABICPPcompound8600, SABICPPcompound, PPcompound 8600, PPcompound8600, PPcompound, 8600, Polypropylene, Unspecified, Polypropylene Unspecified, PP, Unspecified, PP Unspecified, Polypropylene, PP, SABIC, PolypropyleneUnspecified, PPUnspecified, 8600PPcompound
|
|
Generic Name may also be described by the following terms: Polypropilene, Polypropelene.
|
|
Features may also be described by the following terms: High Flow, High Melt, High MFI, High Impact Resistance, Good Processability, Easy Processing, Low Shrinkage, High Stiffness, Low CLTE, Reduced CLTE, Pleasing Surface Appearance.
|
|
Uses may also be described by the following terms: Automotive Applications, Automotive Sector, Automotive Bumper, Automotive Bumpers.
|