Abrasion loss, DIN 53516: 40 mm³ Tosion Test, ASTM D 1043, 20° C: 80 MPa Tosion Test, ASTM D 1043, -20° C: 460 MPa Impact Test, ASTM D 256, -20° C: 4.7 KJ/m²
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: LARIPUR® LPR 6325, LARIPUR LPR 6325, LARIPUR® , LARIPUR, LARIPURLPR6325, LPR 6325, LPR6325, Thermoplastic Polyurethane Elastomer, Thermoplastic Polyurethane Elastomer (Polyester), Thermoplastic Polyurethane Elastomer Polyester, TPU-Polyester, TPUPolyester, TPU:Polyester, TPU/Polyester, TPU+Polyester, TPU_Polyester, TPU Polyester, Thermoplastic Polyurethane, TPU, COIM, ThermoplasticPolyurethaneElastomerPolyester, ThermoplasticPolyurethane, 6325LPR
|
|
Features may also be described by the following terms: Good Tear Strength, Good Toughness, Tough, Low Temperature Toughness, Good Weather Resistance, Weather Resistant.
|