The value listed as Thermal Conductivity, ASTM C177, was tested in accordance with ASTM C518.
Viscosity, 30°C: 700 cps
Density (liquid), 25°C: 1.13 g/cm³
Optical Properties at 351 nm:
- Dp (slope of cure-depth vs. ln(E) curve): 0.142 mm
- Ec (critical exposure): 10 mJ/cm²
- E5 (exposure that gives 0.127 mm (0.005 in) thickness): 24 mJ/cm²
- E10 (exposure that gives 0.254 mm (0.010 in) thickness): 59 mJ/cm²
Tensile Elongation at Break, ASTM D638: 1.8 to 7.8%
Heat Deflection Temperature, ASTM D648: 57 to 61°C
Ash Content, Weight Loss at 1000°C, TGA: 100%