Viscosity, 30°C: 450 cps
Density (liquid), 25°C: 1.13 g/cm³
Optical Properties at 355 nm:
- Dp (slope of cure-depth vs. ln(E) curve): 0.14 mm
- Ec (critical exposure): 10.9 mJ/cm²
- E10 (exposure that gives 0.254 mm (0.010 in) thickness): 65 mJ/cm²
Tensile Strength at Yield, ASTM D638: 30 to 32 MPa
Elongation at Yield, ASTM D638: 15 to 25%
Tensile Modulus, ASTM D638: 1227 to 1462 MPa
Flexural Strength, ASTM D790: 41 to 46 MPa
Flexural Modulus, ASTM D790: 1310 to 1455 MPa
Notched Izod Impact, ASTM D256, Method A: 48 to 53 J/m
HDT, ASTM D648: 52 to 61°C