The value listed as Taber Abrasion Resistance ASTM D1044, was tested in accordance with ASTM D3489 (ISO 4649). Compression Set: postcured for 16 hours @ 230°F, not postcuring will result in higher values. The values listed as, Mold Shirnkage ISO 294-4, were tested in accordance with ISO 2577.
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: Texin® 1193, Texin 1193, Texin® , Texin, Texin1193, 1193, Thermoplastic Polyurethane Elastomer, Thermoplastic Polyurethane Elastomer (Polyether), Thermoplastic Polyurethane Elastomer Polyether, TPU-Polyether, TPUPolyether, TPU:Polyether, TPU/Polyether, TPU+Polyether, TPU_Polyether, TPU Polyether, Thermoplastic Polyurethane, TPU, Bayer, ThermoplasticPolyurethaneElastomerPolyether, ThermoplasticPolyurethane
|
|
Features may also be described by the following terms: Good Abrasion Resistance, Abrasion Resistant, Good Impact Resistance, Good Toughness, Tough, Good Flexibility, Flexible.
|