Tear Strength, ISO 34: 500 lbf/in Compression Set was postcured for 16 hours @230°F, not postcuring will result in higher values. The value listed as Taber Abrasion ASTM D1044, was tested in accordance with ASTM D3489 (ISO 4649). The values listed as, Mold Shirnkage ISO 294-4, were tested in accordance with ISO 2577.
|
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: Texin® 1186, Texin 1186, Texin® , Texin, Texin1186, 1186, Thermoplastic Polyurethane Elastomer, Thermoplastic Polyurethane Elastomer (Polyether), Thermoplastic Polyurethane Elastomer Polyether, TPU-Polyether, TPUPolyether, TPU:Polyether, TPU/Polyether, TPU+Polyether, TPU_Polyether, TPU Polyether, Thermoplastic Polyurethane, TPU, Bayer, ThermoplasticPolyurethaneElastomerPolyether, ThermoplasticPolyurethane
|
|
Features may also be described by the following terms: Good Abrasion Resistance, Abrasion Resistant, Good Flexibility, Flexible, Good Impact Resistance, Good Toughness, Tough.
|
|
Uses may also be described by the following terms: Belts/Belt Repair, Belt Repair, Gaskets, Gasketing, Tubing, Tube, Food Applications.
|