Elmendorf Tear Strength - ASTM D1922 Plastic Test Standard

Share This Page Share This Page  •  Free Access to 80,000 Datasheets

Elmendorf Tear Strength - ASTM D1922

ASTM D1922 Purchase and download the official ASTM D1922 standard today!

The average force required to propagate tearing through a specified length of plastic film or nonrigid sheeting on an Elmendorf-type tear tester.

Rectangular Specimen

Constant Radius Specimen

Constant radius specimens are used for materials that do not tear in a straight line.

Test specimens have a pre-cut slit. Testing is performed using a knife-tipped pendulum. The average force is calculated from the pendulum energy lost while tearing the test specimen. Tear direction is either in the machine direction (MD) or transverse direction (TD).

MD and TD Specimens

Similar Standards


Property information for specific grades of resin are available in the Prospector.
If you already have an account, you can login here or you can register for free, instant access:

Join the IDES Network:   Email Alerts  •  Blog  •  Twitter  •  LinkedIn

Share This Page - Services - Advertise With Us - About IDES - Contact Us NA: 800-788-4668, 307-742-9227  |  EU: 0033 (0) 471 759 577 Chat ©1986- IDES